Polystyrene Nanocomposites after Melt Intercalation

ASTRA Polystrene

Melt intercalation exposes polymers to thermal and shear histories that can induce degradation. An extruded macrocomposite comprising polystyrene and montmorillonite was statically annealed in an O2-rich environment at 250 °C to induce localized chain scission.